An In Vitro Evaluation of the Fracture Resistance of Computer-Aided Design/Computer-Aided Manufacturing Materials for Fixed Partial Dentures

Authors

  • Ajay Pandey Department of Dentistry, Government Medical College and Hospital, Bettiah, Bihar, India.
  • Rachna Kaushik Department of Dentistry, Government Medical College and Hospital, Bettiah, Bihar, India.
  • Lily Tiwari Smile Saver, Bettiah, Bihar, India.

DOI:

https://doi.org/10.21276/apjhs.2026.13.4.35

Keywords:

Computer-aided design/Computer-aided manufacturing, Fixed partial dentures, Fracture resistance, In vitro study, Lithium disilicate, Resin-based CAD/CAM materials, Zirconia-reinforced glass-ceramic

Abstract

Background: The mechanical durability of computer-aided design and computer-aided manufacturing (CAD/CAM) restorative materials is essential for the long-term performance of fixed partial dentures (FPDs). Differences in material composition and microstructure may influence their resistance to fracture under occlusal loading. Aim: The aim of the study is to evaluate and compare the fracture resistance of three CAD/CAM restorative materials used for three-unit FPDs under standardized in vitro conditions. Materials and Methods: The proposed experimental study comprised 30 standardized three-unit FPDs divided equally into three groups (n = 10): Group I, lithium disilicate glass-ceramic; Group II, zirconia-reinforced glass-ceramic; and Group III, resin-based CAD/CAM material. The restorations were designed for cementation onto standardized epoxy resin dies using resin cement. Fracture resistance was assessed using a universal testing machine at a crosshead speed of 1 mm/min, with maximum fracture load expressed in Newtons (N). The illustrative dataset was analyzed using one-way analysis of variance (ANOVA), followed by Tukey’s post hoc test. Statistical significance was set at P < 0.05. Results: In the simulated dataset, Group II exhibited the highest mean fracture resistance (1312.60 ± 83.93 N), followed by Group I (1111.80 ± 82.27 N) and Group III (921.10 ± 75.41 N). One-way ANOVA identified a statistically significant difference among the groups (F = 58.966; P < 0.001). Tukey’s post hoc analysis showed statistically significant differences between all three material pairs (P < 0.001). Conclusion: The illustrative analysis showed the highest mean fracture resistance for zirconia-reinforced glass-ceramic, followed by lithium disilicate glass-ceramic and resin-based CAD/CAM material.

Downloads

Download data is not yet available.

Downloads

Published

2026-11-25

How to Cite

Ajay Pandey, Rachna Kaushik, & Lily Tiwari. (2026). An In Vitro Evaluation of the Fracture Resistance of Computer-Aided Design/Computer-Aided Manufacturing Materials for Fixed Partial Dentures. Asian Pacific Journal of Health Sciences, 13(4), 178–184. https://doi.org/10.21276/apjhs.2026.13.4.35